Adrithia, Giovanno Adnan (2020) PENGARUH BAHAN TAMBAH POLCON® TERHADAP KUAT TEKAN MORTAR. Other thesis, Universitas Katolik Soegijapranata Semarang.
|
Text
15B10007_Giovanno Adnan Adrithia_COVER_a.pdf Download (20MB) | Preview |
|
|
Text
15B10007_Giovanno Adnan Adrithia_BAB I_a.pdf Download (20MB) | Preview |
|
Text
15B10007_Giovanno Adnan Adrithia_BAB II_a.pdf Restricted to Registered users only Download (20MB) |
||
|
Text
15B10007_Giovanno Adnan Adrithia_BAB III_a.pdf Download (20MB) | Preview |
|
|
Text
15B10007_Giovanno Adnan Adrithia_BAB IV_a.pdf Download (20MB) | Preview |
|
|
Text
15B10007_Giovanno Adnan Adrithia_BAB V_a.pdf Download (20MB) | Preview |
|
|
Text
15B10007_Giovanno Adnan Adrithia_DAPUS_a.pdf Download (20MB) | Preview |
|
|
Text
15B10007_Giovanno Adnan Adrithia_LAMP_a.pdf Download (20MB) | Preview |
Abstract
Mortar merupakan material konstruksi yang paling sering di pakai dan diminati karena merupakan bahan dasar yang mudah dibentuk dengan harga yang relatif murah dibandingkan dengan konstruksi lainnya. Pemanfaatan POLCON® sebagai bahan tambah pada campuran mortar sangat bermanfaat ditinjau kuat tekan mortar. Pengujian kuat tekan mortar dilakukan pada umur 7 hari, 14 hari, 28 hari dengan benda uji berbentuk kubus. Dari penelitian ini diketahui bahwa dengan prosentase penambahan POLCON® mortar akan memiliki nilai kuat tekan yang tinggi dibandingkan dengan mortar normal. Nilai kuat tekan beton yang paling tinggi didapat dari komposisi campuran 4% penambahan fly ash yang mencapai nilai 322 Kg/cm2 Mortar is the most frequently used construction material and is in demand because it is a basic material that is easily formed at a relatively cheap price compared to other construction. Utilization of POLCON® as an added ingredient in mortar mixtures is very useful in terms of compressive strength of mortars. Mortar compressive strength testing is done at the age of 7 days, 14 days, 28 days with cube-shaped test specimens. From this study it is known that the percentage of POLCON® mortar addition will have a high compressive strength value compared to normal mortar. The highest concrete compressive strength value obtained from the composition of the mixture of 4% addition of fly ash which reached a value of 322 Kg/cm2
Item Type: | Thesis (Other) |
---|---|
Subjects: | 600 Technology (Applied sciences) > 620 Engineering > 624 Civil engineering > Civil Engineering |
Divisions: | Faculty of Engineering > Department of Civil Engineering |
Depositing User: | mr AM. Pudja Adjie Sudoso |
Date Deposited: | 05 Jan 2021 05:41 |
Last Modified: | 05 Jan 2021 05:41 |
URI: | http://repository.unika.ac.id/id/eprint/23005 |
Actions (login required)
View Item |